    矿化碳酸钙晶型对高添加PVC复合材料力学与热学性能的影响

    Effect of calcium carbonate crystal form on the mechanical and thermal properties of highly filled PVC composites

    • 摘要: 为探索大宗固废磷石膏矿化制备的CaCO3产品在聚合物体系中的应用潜力,以通过调控矿化工艺合成并经疏水改性的纳米方解石与文石型CaCO3为填料,以聚氯乙烯(PVC)为基体,制备了一系列CaCO3/PVC复合材料。重点考察了CaCO3晶型与添加量对复合材料力学性能及热稳定性的影响。结果表明:当填料添加量达40 phr(parts per hundred parts of resin,即每百份树脂中的质量份数)时,相比于纯PVC基体(拉伸强度17.1 MPa,断裂伸长率488%),方解石体系的拉伸强度降至15.9 MPa;而文石体系凭借高长径比优势,拉伸强度维持在17.6 MPa,断裂伸长率升至531%。该力学指标不仅与市售商业纳米CaCO3(17.8 MPa,518%)综合效能相当,且远超电缆料国标(GB/T 8815—2008)安全阈值(拉伸强度10.0~12.5 MPa,断裂伸长率≥150%)。热分析结果表明,文石体系的起始热分解温度较纯树脂有所提高,延缓了PVC热降解过程。定向调控合成的矿化文石型CaCO3可突破聚合物高填充引发的力学劣化瓶颈,为工业固废磷石膏的高值化、规模化利用及塑料体系的降本增效提供技术支撑。

       

      Abstract: To explore the application potential of CaCO3 products prepared by the mineralization of bulk phosphogypsum solid waste in polymer systems, a series of CaCO3/PVC composites were prepared using nano-calcite and nano-aragonite (synthesized in the laboratory by adjusting mineralization process and subsequently hydrophobic-modified) as fillers, with polyvinyl chloride (PVC) as the matrix. The effects of CaCO3 crystal polymorphs and loading amounts on the mechanical properties and thermal stability of the composites were primarily investigated. The results indicate that at a filler loading of 40 phr (parts per hundred parts of resin), compared to the pure PVC matrix (tensile strength of 17.1 MPa, elongation at break of 488%), the tensile strength of the calcite-filled system decreased to 15.9 MPa. Conversely, benefiting from its high aspect ratio advantage, the aragonite-filled system maintained a tensile strength of 17.6 MPa and exhibited an increased elongation at break of 531%. These mechanical indicators are highly comparable to those of commercial nano-CaCO3 (17.8 MPa, 518%) and significantly exceed the safety thresholds specified in the GB/T 8815—2008 national standard for cable compounds (tensile strength 10.0~12.5 MPa, elongation at break ≥ 150%). Thermal analysis results indicate that the initial thermal decomposition temperature of the aragonite system was elevated compared to the pure resin, delaying the thermal degradation process of PVC. Directionally regulated synthetic mineralized aragonite can break through the bottleneck of mechanical deterioration caused by high polymer filling, thereby providing technical support for the high-value and large-scale utilization of industrial solid waste phosphogypsum and for reducing costs and improving efficiency in plastic systems.

       

    /

    返回文章
    返回